High temperature corrosion behaviour of austenitic stainless steel with CaCO₃ and MgCO₃ deposit
The high temperature corrosion behaviour of austenitic stainless steel was studied at 850°C, 900°C, 950°C and 1000°C for 24 to 120 hr exposure time with CaCO₃ and MgCO₃ deposit. Two commercial available austenitic stainless steel grade of AISI 304 and AISI 316L were selected. Austenitic stainless...
Saved in:
主要作者: | Habsah, Md Ishak |
---|---|
格式: | Thesis |
語言: | English |
主題: | |
在線閱讀: | http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/33276/1/page%201-24.pdf http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/33276/2/Full%20text.pdf |
標簽: |
添加標簽
沒有標簽, 成為第一個標記此記錄!
|
相似書籍
-
Stress corrosion cracking behavior of austenitic stainless steels in natrium chloride solutions
由: Samir Milad, Elsariti -
Hybrid process of low temperature nitriding-carburizing for austenitic stainless steel /
由: Triwiyanto, Askar
出版: (2010) -
Prediction of steam-side oxide scale growth of austenitic stainless steel alloy in superheater and reheater tubes /
由: Ragupathy Mohan
出版: (2013) -
Investigation on the mechanical properties and microstructure analysis of micro-resistance spot welding between stainless steel 316L and Tl-6AL-4V /
由: Muhammad Safwan Mohd. Mansor
出版: (2020) -
Microstructural evolution and mechanical properties of magnesium alloy/austenitic stainless steel joints produced by resistance spot welding techniques /
由: Manladan, Sunusi Marwana
出版: (2017)