1
-
2by Md Yusuf, Muhammad Yusri“.... The fillers ratio was fixed in the range of (25 up to 65 wt%) G, (10 up to 30 wt%) CB and (5 up to 25 wt%) Fe...”
Published 2018
Get full text
Get full text
Thesis -
3
-
4by Mansoor, Mohd Sufriansyah“... (0.1mm-1.5mm). RSM using Box-Behnken was used to determine the most influential paremeters affected...”
Published 2019
Get full text
Get full text
Thesis -
5
-
6by Abdul Rahim, Mohd Aidil Shah“... finding on Ml and M3 which provide an increase in its bulk hardness from 51.5HRC to 52HRC (Ml) and 52.6HRC...”
Published 2019
Get full text
Get full text
Thesis -
7
-
8by Mat Noor, Noraina Alia“... and optimization between kenaf fibre content (-5.00 wt. %; +35.00 wt. %), stirring time (-10.00 minutes; +50.00...”
Published 2019
Get full text
Get full text
Thesis -
9by Abd Yazid, Nurul Shuhadah“... is to investigate the influences of solvent with ethanol (E16 and E8) and without ethanol (E0) at five and ten...”
Published 2020
Get full text
Get full text
Thesis -
10
-
11by Raja Seman, Raja Noor Amalina“... at 14.3°, 33.8°, and 57.5° are attributed to the (002), (100), and (110) plane of MoS2 crystal. From Raman...”
Published 2019
Get full text
Get full text
Thesis -
12
-
13
-
14
-
15
-
16
-
17by Harun, Nurul Hatiqah“... mm) and part angle (22.5°, 45°, 67,5°) have been studied. A total of 29 numbers of experiments had...”
Published 2019
Get full text
Get full text
Thesis -
18
-
19by Mohamad Yatim, Norazlina“... based on a five-level Central Composite Design consisting of f-MWCNTs amount between 0.10–0.60wt...”